@article{Dmello2016261,
title = "Cost-driven materials selection criteria for redox flow battery electrolytes ",
journal = "Journal of Power Sources ",
volume = "330",
number = "",
pages = "261 - 272",
year = "2016",
note = "",
issn = "0378-7753",
doi = "http://dx.doi.org/10.1016/j.jpowsour.2016.08.129",
url = "http://www.sciencedirect.com/science/article/pii/S0378775316311491",
author = "Rylan Dmello and Jarrod D. Milshtein and Fikile R. Brushett and Kyle C. Smith",
keywords = "Redox flow battery",
keywords = "Electrolyte",
keywords = "Techno-economic model",
keywords = "Energy storage "
}
