@article{Qu201556,
title = "The Electrolyte Genome project: A big data approach in battery materials discovery ",
journal = "Computational Materials Science ",
volume = "103",
number = "",
pages = "56 - 67",
year = "2015",
note = "",
issn = "0927-0256",
doi = "http://dx.doi.org/10.1016/j.commatsci.2015.02.050",
url = "http://www.sciencedirect.com/science/article/pii/S0927025615001512",
author = "Xiaohui Qu and Anubhav Jain and Nav Nidhi Rajput and Lei Cheng and Yong Zhang and Shyue Ping Ong and Miriam Brafman and Edward Maginn and Larry A. Curtiss and Kristin A. Persson",
keywords = "High-throughput",
keywords = "Battery",
keywords = "DFT",
keywords = "Ionization potential",
keywords = "Electron affinity",
keywords = "IP/EA",
keywords = "Dissociation constants",
keywords = "Electrolyte "
}
