@article{doi:10.1021/jz502319n,
author = {Lei Cheng and Rajeev S. Assary and Xiaohui Qu and Anubhav Jain and Shyue Ping Ong and Nav Nidhi Rajput and Kristin Persson and Larry A. Curtiss},
title = {Accelerating Electrolyte Discovery for Energy Storage with High-Throughput Screening},
journal = {The Journal of Physical Chemistry Letters},
volume = {6},
number = {2},
pages = {283-291},
year = {2015},
doi = {10.1021/jz502319n},
    note ={PMID: 26263464},
URL = {http://dx.doi.org/10.1021/jz502319n},
eprint = {http://dx.doi.org/10.1021/jz502319n}
}