Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.013 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.013 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.71 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSr |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinIm3m [229] |
Hall-I 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | elastic energy [meV] | MCIA† [Å2] |
---|---|---|---|---|
Ni (mp-23) | <1 1 0> | <1 1 0> | 0.001 | 191.7 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 0.001 | 274.0 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 0.001 | 90.4 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 0.002 | 180.8 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 0.006 | 203.4 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 0> | 0.008 | 226.0 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <1 0 0> | 0.008 | 113.0 |
YAlO3 (mp-3792) | <0 1 0> | <1 1 0> | 0.010 | 351.5 |
GaP (mp-2490) | <1 1 0> | <1 1 0> | 0.010 | 127.8 |
SiC (mp-11714) | <0 0 1> | <1 1 1> | 0.010 | 156.6 |
LiGaO2 (mp-5854) | <1 0 0> | <1 1 0> | 0.010 | 319.6 |
GaP (mp-2490) | <1 1 1> | <1 1 1> | 0.011 | 156.6 |
SiC (mp-7631) | <0 0 1> | <1 1 1> | 0.012 | 156.6 |
Si (mp-149) | <1 1 0> | <1 1 0> | 0.014 | 127.8 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 0.014 | 293.8 |
Si (mp-149) | <1 1 1> | <1 1 1> | 0.015 | 156.6 |
NdGaO3 (mp-3196) | <0 1 0> | <1 1 0> | 0.015 | 127.8 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 0.016 | 127.8 |
CeO2 (mp-20194) | <1 1 1> | <1 1 1> | 0.017 | 156.6 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 0.018 | 117.4 |
YAlO3 (mp-3792) | <1 1 0> | <1 0 0> | 0.024 | 113.0 |
CaF2 (mp-2741) | <1 1 0> | <1 1 0> | 0.025 | 127.8 |
CaF2 (mp-2741) | <1 1 1> | <1 1 1> | 0.027 | 156.6 |
Te2Mo (mp-602) | <1 0 1> | <1 1 0> | 0.028 | 223.7 |
AlN (mp-661) | <0 0 1> | <1 1 0> | 0.028 | 127.8 |
Al2O3 (mp-1143) | <0 0 1> | <1 0 0> | 0.029 | 158.2 |
C (mp-66) | <1 1 1> | <1 1 1> | 0.030 | 156.6 |
LaAlO3 (mp-2920) | <0 0 1> | <1 1 0> | 0.031 | 127.8 |
CaCO3 (mp-3953) | <0 0 1> | <1 1 1> | 0.036 | 156.6 |
Ga2O3 (mp-886) | <1 0 0> | <1 1 0> | 0.039 | 287.6 |
LaAlO3 (mp-2920) | <1 1 1> | <1 1 0> | 0.039 | 127.8 |
NdGaO3 (mp-3196) | <1 0 1> | <1 0 0> | 0.043 | 271.2 |
KP(HO2)2 (mp-23959) | <1 0 0> | <1 0 0> | 0.043 | 113.0 |
SrTiO3 (mp-4651) | <1 0 1> | <1 0 0> | 0.045 | 271.2 |
Cu (mp-30) | <1 1 1> | <1 1 1> | 0.045 | 156.6 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 0 0> | 0.048 | 226.0 |
WSe2 (mp-1821) | <1 0 0> | <1 0 0> | 0.049 | 203.4 |
TePb (mp-19717) | <1 1 1> | <1 0 0> | 0.050 | 226.0 |
NdGaO3 (mp-3196) | <1 0 0> | <1 1 0> | 0.053 | 351.5 |
MgAl2O4 (mp-3536) | <1 1 0> | <1 1 0> | 0.059 | 95.9 |
C (mp-48) | <1 0 1> | <1 1 0> | 0.059 | 159.8 |
MgAl2O4 (mp-3536) | <1 1 1> | <1 1 1> | 0.063 | 117.4 |
C (mp-66) | <1 0 0> | <1 0 0> | 0.065 | 113.0 |
MgF2 (mp-1249) | <1 1 1> | <1 1 1> | 0.065 | 274.0 |
CdTe (mp-406) | <1 1 1> | <1 0 0> | 0.065 | 226.0 |
ZrO2 (mp-2858) | <0 1 0> | <1 1 0> | 0.066 | 255.6 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 0.066 | 95.9 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 0.070 | 180.8 |
LiF (mp-1138) | <1 1 1> | <1 1 1> | 0.071 | 117.4 |
InSb (mp-20012) | <1 1 1> | <1 0 0> | 0.071 | 226.0 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
14 | 11 | 11 | 0 | 0 | 0 |
11 | 14 | 11 | 0 | 0 | 0 |
11 | 11 | 14 | 0 | 0 | 0 |
0 | 0 | 0 | 14 | 0 | 0 |
0 | 0 | 0 | 0 | 14 | 0 |
0 | 0 | 0 | 0 | 0 | 14 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
224.5 | -97.8 | -97.8 | 0 | 0 | 0 |
-97.8 | 224.5 | -97.8 | 0 | 0 | 0 |
-97.8 | -97.8 | 224.5 | 0 | 0 | 0 |
0 | 0 | 0 | 70.5 | 0 | 0 |
0 | 0 | 0 | 0 | 70.5 | 0 |
0 | 0 | 0 | 0 | 0 | 70.5 |
Shear Modulus GV9 GPa |
Bulk Modulus KV12 GPa |
Shear Modulus GR3 GPa |
Bulk Modulus KR12 GPa |
Shear Modulus GVRH6 GPa |
Bulk Modulus KVRH12 GPa |
Elastic Anisotropy8.70 |
Poisson's Ratio0.27 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
HoInAg2 (mp-30342) | 0.0000 | 0.000 | 3 |
HfCuHg2 (mp-30582) | 0.0000 | 0.232 | 3 |
LiNi2Sn (mp-13915) | 0.0000 | 0.000 | 3 |
AlCrCu2 (mp-16494) | 0.0000 | 0.160 | 3 |
ScAlNi2 (mp-10898) | 0.0000 | 0.000 | 3 |
LiMgSnPd (mp-7555) | 0.0000 | 0.000 | 4 |
LiMgSnAu (mp-7554) | 0.0000 | 0.088 | 4 |
VFeCoGe (mp-1063914) | 0.0000 | 0.000 | 4 |
LiMgSbPd (mp-10179) | 0.0000 | 0.096 | 4 |
LiMgSnPt (mp-11806) | 0.0000 | 0.000 | 4 |
Li3Tl (mp-7396) | 0.0000 | 0.000 | 2 |
Li3Bi (mp-23222) | 0.0000 | 0.000 | 2 |
BiF3 (mp-23301) | 0.0000 | 0.271 | 2 |
GdMg3 (mp-20534) | 0.0000 | 0.042 | 2 |
DyMg3 (mp-1546) | 0.0000 | 0.000 | 2 |
Yb (mp-71) | 0.0000 | 0.017 | 1 |
Dy (mp-10751) | 0.0000 | 0.147 | 1 |
Li (mp-135) | 0.0000 | 0.005 | 1 |
Na (mp-127) | 0.0000 | 0.002 | 1 |
La (mp-10023) | 0.0000 | 0.134 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sr_sv |
Final Energy/Atom-1.6764 eV |
Corrected Energy-1.6764 eV
Uncorrected energy = -1.6764 eV
Corrected energy = -1.6764 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)