Final Magnetic Moment0.374 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.633 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.054 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.20 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiTiCrO4 + Li2TiO3 + Li4Ti5O12 + CrWO4 + W |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCm [8] |
HallC 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <0 0 1> | 123.5 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 234.9 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 308.8 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 172.1 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 176.1 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 293.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 247.0 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 247.0 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 308.8 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 176.1 |
LiNbO3 (mp-3731) | <1 0 1> | <0 0 1> | 308.8 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 176.1 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 123.5 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 61.8 |
BN (mp-984) | <0 0 1> | <1 0 0> | 176.1 |
BN (mp-984) | <1 1 0> | <1 1 0> | 235.2 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 185.3 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 1> | 258.1 |
Al (mp-134) | <1 0 0> | <0 0 1> | 247.0 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 234.9 |
LiTaO3 (mp-3666) | <1 0 1> | <0 0 1> | 308.8 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 234.9 |
SiC (mp-7631) | <1 0 1> | <0 1 1> | 238.3 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 185.3 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 185.3 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 308.8 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 123.5 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 123.5 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 61.8 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 308.8 |
C (mp-66) | <1 1 1> | <1 0 0> | 176.1 |
C (mp-66) | <1 0 0> | <1 0 1> | 258.1 |
C (mp-66) | <1 1 0> | <1 0 0> | 176.1 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 176.1 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 247.0 |
Mg (mp-153) | <1 0 1> | <1 0 1> | 172.1 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 176.1 |
BaTiO3 (mp-5986) | <0 0 1> | <1 0 0> | 234.9 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 247.0 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 247.0 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 247.0 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 293.6 |
BaTiO3 (mp-5986) | <1 0 1> | <1 0 0> | 117.4 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 176.1 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 123.5 |
Ga2O3 (mp-886) | <0 1 0> | <1 0 0> | 293.6 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 185.3 |
Ga2O3 (mp-886) | <1 1 0> | <1 0 0> | 293.6 |
Ga2O3 (mp-886) | <1 0 1> | <1 0 0> | 234.9 |
Au (mp-81) | <1 0 0> | <1 0 0> | 176.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li(FeO2)2 (mp-771571) | 0.1650 | 0.665 | 3 |
Fe19Co5O32 (mp-762884) | 0.1707 | 0.044 | 3 |
Mn19Fe17O48 (mp-706492) | 0.1873 | 0.068 | 3 |
LiTi2O4 (mp-776170) | 0.1824 | 0.042 | 3 |
Co2SnO4 (mp-706412) | 0.1487 | 0.053 | 3 |
Li4Mn3Fe5O16 (mp-772388) | 0.1045 | 0.048 | 4 |
Li2Ti3NbO8 (mp-775796) | 0.1073 | 0.083 | 4 |
Li2Cr3TeO8 (mp-778785) | 0.1285 | 0.023 | 4 |
Li2Fe3SnO8 (mp-773163) | 0.0967 | 0.328 | 4 |
Li4Cr3Sn5O16 (mp-773182) | 0.1036 | 0.028 | 4 |
Fe3O4 (mp-542433) | 0.2642 | 0.075 | 2 |
Fe3O4 (mp-650112) | 0.2575 | 0.060 | 2 |
Fe3O4 (mp-715558) | 0.2739 | 0.785 | 2 |
Fe3O4 (mp-716052) | 0.2767 | 0.781 | 2 |
Fe3O4 (mp-715811) | 0.2750 | 0.037 | 2 |
Li4Ti3Cr3(SnO8)2 (mp-776780) | 0.0724 | 0.138 | 5 |
Li4Cr3Co3(SbO8)2 (mp-762055) | 0.1093 | 0.084 | 5 |
Li4Mn3Fe3(CuO8)2 (mp-767314) | 0.1079 | 5.833 | 5 |
Li4Cr3Fe3(TeO8)2 (mp-773518) | 0.1137 | 0.054 | 5 |
Li4Fe3Co3(SnO8)2 (mp-793779) | 0.1164 | 0.070 | 5 |
Li3MnFeCo(PO4)3 (mp-764931) | 0.7064 | 0.017 | 6 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.6951 | 0.014 | 6 |
Li3MnFeCo(PO4)3 (mp-764869) | 0.6997 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764969) | 0.7006 | 0.057 | 6 |
Li3MnFeCo(PO4)3 (mp-764870) | 0.7046 | 0.466 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eVW: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv Ti_pv Cr_pv W_pv O |
Final Energy/Atom-7.6189 eV |
Corrected Energy-239.1952 eV
Uncorrected energy = -213.3302 eV
Composition-based energy adjustment (-0.687 eV/atom x 16.0 atoms) = -10.9920 eV
Composition-based energy adjustment (-1.999 eV/atom x 3.0 atoms) = -5.9970 eV
Composition-based energy adjustment (-4.438 eV/atom x 2.0 atoms) = -8.8760 eV
Corrected energy = -239.1952 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)