Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.413 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.42 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap4.032 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP212121 [19] |
HallP 2ac 2ab |
Point Group222 |
Crystal Systemorthorhombic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaTe (mp-542812) | <0 0 1> | <1 1 0> | 297.8 |
Al2O3 (mp-1143) | <1 0 0> | <1 0 1> | 252.3 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 50.5 |
YAlO3 (mp-3792) | <0 1 0> | <0 0 1> | 78.1 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 286.5 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 52.1 |
Mg (mp-153) | <1 1 0> | <1 0 0> | 86.4 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 286.5 |
GdScO3 (mp-5690) | <0 1 1> | <0 1 0> | 164.0 |
LiAlO2 (mp-3427) | <1 0 1> | <1 0 0> | 43.2 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 234.4 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 260.5 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 156.3 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 78.1 |
GaTe (mp-542812) | <1 0 0> | <1 1 0> | 178.7 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 130.2 |
MgF2 (mp-1249) | <0 0 1> | <0 1 0> | 327.9 |
Mg (mp-153) | <1 0 0> | <1 0 1> | 50.5 |
TbScO3 (mp-31119) | <0 0 1> | <0 0 1> | 286.5 |
BN (mp-984) | <0 0 1> | <0 0 1> | 130.2 |
TiO2 (mp-2657) | <0 0 1> | <0 1 0> | 327.9 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 234.4 |
MoSe2 (mp-1634) | <0 0 1> | <1 1 0> | 238.2 |
WSe2 (mp-1821) | <0 0 1> | <1 1 0> | 238.2 |
WS2 (mp-224) | <1 1 1> | <1 1 0> | 238.2 |
MoSe2 (mp-1634) | <1 0 1> | <1 0 0> | 259.2 |
GaSe (mp-1943) | <0 0 1> | <1 1 0> | 238.2 |
GaP (mp-2490) | <1 0 0> | <0 1 1> | 242.8 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 82.0 |
TbScO3 (mp-31119) | <0 1 1> | <0 1 0> | 164.0 |
Al2O3 (mp-1143) | <1 1 0> | <1 0 0> | 216.0 |
ZnO (mp-2133) | <1 0 0> | <0 0 1> | 52.1 |
ZrO2 (mp-2858) | <1 0 1> | <1 0 0> | 43.2 |
CaF2 (mp-2741) | <1 0 0> | <0 1 1> | 242.8 |
LiGaO2 (mp-5854) | <1 0 1> | <1 1 0> | 178.7 |
MgAl2O4 (mp-3536) | <1 1 0> | <0 1 0> | 287.0 |
NdGaO3 (mp-3196) | <1 1 0> | <0 1 1> | 242.8 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 205.0 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 234.4 |
CaCO3 (mp-3953) | <1 0 0> | <0 0 1> | 260.5 |
C (mp-48) | <1 1 1> | <1 1 0> | 238.2 |
ZrO2 (mp-2858) | <1 0 -1> | <0 0 1> | 182.3 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 1> | 340.0 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 260.5 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 172.8 |
C (mp-48) | <1 0 0> | <0 0 1> | 78.1 |
SiC (mp-8062) | <1 0 0> | <0 1 1> | 97.1 |
CdWO4 (mp-19387) | <0 1 1> | <1 1 1> | 325.0 |
Ge (mp-32) | <1 1 0> | <1 1 0> | 238.2 |
TeO2 (mp-2125) | <1 0 0> | <0 0 1> | 286.5 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
18 | 5 | 10 | 0 | 0 | 0 |
5 | 18 | 5 | 0 | 0 | 0 |
10 | 5 | 14 | 0 | 0 | 0 |
0 | 0 | 0 | 7 | 0 | 0 |
0 | 0 | 0 | 0 | 12 | 0 |
0 | 0 | 0 | 0 | 0 | 9 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
99.3 | -8.7 | -70 | 0 | 0 | 0 |
-8.7 | 61.4 | -14.2 | 0 | 0 | 0 |
-70 | -14.2 | 128.6 | 0 | 0 | 0 |
0 | 0 | 0 | 140.6 | 0 | 0 |
0 | 0 | 0 | 0 | 83.7 | 0 |
0 | 0 | 0 | 0 | 0 | 115 |
Shear Modulus GV8 GPa |
Bulk Modulus KV10 GPa |
Shear Modulus GR6 GPa |
Bulk Modulus KR10 GPa |
Shear Modulus GVRH7 GPa |
Bulk Modulus KVRH10 GPa |
Elastic Anisotropy1.43 |
Poisson's Ratio0.22 |
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | 0.03232 | 0.00000 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | -0.19941 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.06001 |
Piezoelectric Modulus ‖eij‖max0.19941 C/m2 |
Crystallographic Direction vmax |
---|
0.00000 |
0.00000 |
1.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
2.93 | 0.00 | 0.00 |
0.00 | 2.91 | 0.00 |
0.00 | 0.00 | 2.84 |
Dielectric Tensor εij (total) |
||
---|---|---|
15.44 | 0.00 | 0.00 |
0.00 | 41.59 | 0.00 |
0.00 | 0.00 | 12.83 |
Polycrystalline dielectric constant
εpoly∞
2.89
|
Polycrystalline dielectric constant
εpoly
23.28
|
Refractive Index n1.70 |
Potentially ferroelectric?Unknown |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ge_d F |
Final Energy/Atom-4.8989 eV |
Corrected Energy-62.4823 eV
Uncorrected energy = -58.7863 eV
Composition-based energy adjustment (-0.462 eV/atom x 8.0 atoms) = -3.6960 eV
Corrected energy = -62.4823 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)