Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.817 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.017 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.65 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCeO2 + ZrO2 |
Band Gap1.940 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 0 -1> | 251.6 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 72.8 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 324.0 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 277.7 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 231.4 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 268.9 |
SiO2 (mp-6930) | <1 0 1> | <1 0 -1> | 251.6 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 201.6 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 218.3 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 -1> | 235.4 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 -1> | 251.6 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 1> | 253.9 |
CdS (mp-672) | <0 0 1> | <1 -1 0> | 295.3 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 291.1 |
LiF (mp-1138) | <1 0 0> | <1 1 -1> | 248.3 |
LiF (mp-1138) | <1 1 1> | <0 1 -1> | 235.4 |
AlN (mp-661) | <0 0 1> | <1 -1 0> | 295.3 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 138.9 |
GaAs (mp-2534) | <1 0 0> | <1 -1 1> | 259.7 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 201.6 |
GaSe (mp-1943) | <1 0 0> | <1 -1 -1> | 263.1 |
GaN (mp-804) | <1 1 1> | <1 0 -1> | 251.6 |
BN (mp-984) | <0 0 1> | <0 0 1> | 231.4 |
BN (mp-984) | <1 1 0> | <1 0 -1> | 167.7 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 138.9 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 291.1 |
Al (mp-134) | <1 1 0> | <0 1 1> | 253.9 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 134.4 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 277.7 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 134.4 |
ZnSe (mp-1190) | <1 0 0> | <1 -1 1> | 259.7 |
KTaO3 (mp-3614) | <1 0 0> | <1 -1 1> | 259.7 |
CdS (mp-672) | <1 0 0> | <1 1 1> | 262.5 |
TeO2 (mp-2125) | <0 0 1> | <1 -1 0> | 221.5 |
LiF (mp-1138) | <1 1 0> | <0 1 -1> | 235.4 |
Te2W (mp-22693) | <0 0 1> | <1 1 1> | 131.3 |
YVO4 (mp-19133) | <0 0 1> | <1 0 -1> | 251.6 |
Fe3O4 (mp-19306) | <1 1 0> | <0 1 0> | 201.6 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 324.0 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 277.7 |
Ag (mp-124) | <1 0 0> | <1 1 1> | 262.5 |
Ag (mp-124) | <1 1 1> | <0 1 -1> | 235.4 |
GaSe (mp-1943) | <0 0 1> | <1 0 -1> | 251.6 |
GaSe (mp-1943) | <1 0 1> | <0 0 1> | 138.9 |
C (mp-66) | <1 1 0> | <0 1 0> | 201.6 |
BN (mp-984) | <1 0 0> | <1 -1 -1> | 175.4 |
GdScO3 (mp-5690) | <1 0 0> | <0 1 0> | 134.4 |
Mg (mp-153) | <0 0 1> | <1 0 0> | 291.1 |
MoS2 (mp-1434) | <1 0 0> | <1 -1 -1> | 263.1 |
Al (mp-134) | <1 0 0> | <1 -1 1> | 259.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Zr11VO24 (mp-861249) | 0.2466 | 0.021 | 3 |
CeZr7O16 (mp-752503) | 0.0930 | 0.024 | 3 |
Zr7VO16 (mp-861179) | 0.2586 | 0.027 | 3 |
NbNO (mp-781710) | 0.3273 | 0.025 | 3 |
Zr15VO32 (mp-765884) | 0.1523 | 0.015 | 3 |
Li3NbOF6 (mp-769384) | 0.7254 | 0.046 | 4 |
ZrO2 (mp-2858) | 0.2353 | 0.000 | 2 |
HfO2 (mp-775757) | 0.2811 | 0.010 | 2 |
HfO2 (mp-352) | 0.2475 | 0.000 | 2 |
ZrO2 (mp-776404) | 0.2795 | 0.009 | 2 |
TiO2 (mp-430) | 0.3959 | 0.065 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ce Zr_sv O |
Final Energy/Atom-9.4237 eV |
Corrected Energy-355.7418 eV
Uncorrected energy = -339.2538 eV
Composition-based energy adjustment (-0.687 eV/atom x 24.0 atoms) = -16.4880 eV
Corrected energy = -355.7418 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)