Final Magnetic Moment79.863 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.017 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.014 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.14 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2Mn3CuO8 + Li8Mn13Cr3O32 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCm [8] |
HallC 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 243.1 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 243.1 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 243.1 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 303.8 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 243.1 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 121.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 243.1 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 303.8 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 121.5 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 121.5 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 60.8 |
BN (mp-984) | <0 0 1> | <0 0 1> | 303.8 |
LiNbO3 (mp-3731) | <1 0 1> | <0 0 1> | 303.8 |
Al (mp-134) | <1 0 0> | <0 0 1> | 243.1 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 303.8 |
TeO2 (mp-2125) | <1 0 1> | <0 0 1> | 243.1 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 121.5 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 182.3 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 60.8 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 182.3 |
LiTaO3 (mp-3666) | <1 0 1> | <0 0 1> | 303.8 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 303.8 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 303.8 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 303.8 |
C (mp-66) | <1 0 0> | <0 0 1> | 303.8 |
C (mp-66) | <1 1 1> | <0 0 1> | 182.3 |
C (mp-66) | <1 1 0> | <0 0 1> | 182.3 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 243.1 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 243.1 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 303.8 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 182.3 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 243.1 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 243.1 |
TbScO3 (mp-31119) | <1 0 0> | <0 0 1> | 243.1 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 243.1 |
BaTiO3 (mp-5986) | <1 0 1> | <0 0 1> | 303.8 |
MoSe2 (mp-1634) | <1 1 0> | <0 0 1> | 182.3 |
MoSe2 (mp-1634) | <1 1 1> | <0 0 1> | 182.3 |
Ga2O3 (mp-886) | <1 1 0> | <0 0 1> | 303.8 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 182.3 |
Au (mp-81) | <1 1 0> | <0 0 1> | 121.5 |
C (mp-48) | <0 0 1> | <0 0 1> | 303.8 |
WSe2 (mp-1821) | <1 0 0> | <0 0 1> | 303.8 |
WSe2 (mp-1821) | <1 1 0> | <0 0 1> | 182.3 |
CaCO3 (mp-3953) | <1 0 0> | <0 0 1> | 182.3 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 60.8 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 60.8 |
Ge (mp-32) | <1 0 0> | <0 0 1> | 243.1 |
Fe2O3 (mp-24972) | <0 0 1> | <0 0 1> | 182.3 |
Au (mp-81) | <1 1 1> | <0 0 1> | 60.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mn(FeO2)2 (mp-697842) | 0.1148 | 0.105 | 3 |
Li6Mn9O20 (mp-868928) | 0.1237 | 0.004 | 3 |
MgMn2O4 (mvc-5228) | 0.1018 | 1.184 | 3 |
Mn9(Cu3O10)2 (mp-705729) | 0.1078 | 0.784 | 3 |
Ca(MoO2)2 (mvc-10204) | 0.0989 | 0.661 | 3 |
Li5Mn8Fe11O32 (mp-771896) | 0.1221 | 0.048 | 4 |
Li2MnNi3O8 (mp-777117) | 0.0994 | 0.080 | 4 |
Li2V3CoO8 (mp-774950) | 0.1035 | 0.207 | 4 |
Li2Fe3CoO8 (mp-762595) | 0.1247 | 0.559 | 4 |
Li2FeNi3O8 (mp-776318) | 0.1242 | 0.162 | 4 |
Fe3O4 (mp-715491) | 0.2973 | 0.017 | 2 |
Fe3O4 (mp-542433) | 0.2979 | 0.075 | 2 |
Fe3O4 (mp-650112) | 0.2782 | 0.060 | 2 |
Fe3O4 (mp-31770) | 0.3066 | 0.017 | 2 |
Fe3O4 (mp-715558) | 0.3185 | 0.785 | 2 |
Li4Fe3Cu3(SbO8)2 (mp-764385) | 0.2215 | 6.460 | 5 |
Li4Ti3Cr3(WO8)2 (mp-773537) | 0.2142 | 0.054 | 5 |
Li4Cr3Fe3(TeO8)2 (mp-773518) | 0.2159 | 0.054 | 5 |
Li4Mn3Cr3(CuO8)2 (mp-765456) | 0.2061 | 0.069 | 5 |
TaTi9Al3Zn23O48 (mp-695545) | 0.2087 | 0.054 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eVCr: 3.7 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv Cr_pv Cu_pv O |
Final Energy/Atom-6.7544 eV |
Corrected Energy-743.0967 eV
Uncorrected energy = -661.9317 eV
Composition-based energy adjustment (-0.687 eV/atom x 56.0 atoms) = -38.4720 eV
Composition-based energy adjustment (-1.668 eV/atom x 22.0 atoms) = -36.6960 eV
Composition-based energy adjustment (-1.999 eV/atom x 3.0 atoms) = -5.9970 eV
Corrected energy = -743.0967 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)