Final Magnetic Moment0.514 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.074 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.785 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.91 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToFe3O4 |
Band Gap0.006 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3m [166] |
Hall-R 3 2" |
Point Group2/m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 222.7 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 222.7 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 286.3 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 127.2 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 222.7 |
BaF2 (mp-1029) | <1 1 1> | <1 0 1> | 286.1 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 222.7 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 254.5 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 286.3 |
SiO2 (mp-6930) | <0 0 1> | <1 0 1> | 286.1 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 254.5 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 222.7 |
InAs (mp-20305) | <1 0 0> | <1 0 1> | 190.7 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 222.7 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 269.7 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 286.3 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 254.5 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 349.9 |
YVO4 (mp-19133) | <0 0 1> | <1 1 1> | 158.9 |
Te2Mo (mp-602) | <1 1 1> | <1 0 1> | 95.4 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 31.8 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 222.7 |
Te2Mo (mp-602) | <1 0 1> | <1 0 1> | 286.1 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 159.0 |
GaSe (mp-1943) | <1 0 0> | <1 0 0> | 269.7 |
BN (mp-984) | <1 0 1> | <0 0 1> | 222.7 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 127.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 222.7 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 95.4 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 222.7 |
BN (mp-984) | <0 0 1> | <0 0 1> | 286.3 |
BN (mp-984) | <1 0 0> | <0 0 1> | 349.9 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 1> | 286.1 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 349.9 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 286.3 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 95.4 |
LiTaO3 (mp-3666) | <1 0 0> | <0 0 1> | 286.3 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 127.2 |
CdTe (mp-406) | <1 1 1> | <0 0 1> | 222.7 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 222.7 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 89.9 |
SiC (mp-7631) | <1 1 0> | <1 1 0> | 155.7 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 349.9 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 31.8 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 222.7 |
C (mp-66) | <1 1 1> | <1 0 1> | 286.1 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 127.2 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 159.0 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 349.9 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 254.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Fe2CoO4 (mp-691111) | 0.1228 | 0.072 | 3 |
Zn9Fe21O40 (mp-778406) | 0.0938 | 0.103 | 3 |
Fe9Cu3O16 (mp-705842) | 0.1212 | 0.124 | 3 |
Mg5Fe19O32 (mp-764436) | 0.0723 | 0.068 | 3 |
Zn(FeO2)2 (mp-34296) | 0.1299 | 0.052 | 3 |
Li4V2OF7 (mp-765046) | 0.1743 | 0.054 | 4 |
LiZn6Fe17O32 (mp-771348) | 0.1390 | 0.091 | 4 |
LiZn4Fe13O24 (mp-769606) | 0.1509 | 0.084 | 4 |
Li3Mg2Fe19O32 (mp-771996) | 0.1630 | 0.068 | 4 |
LiZn2Fe9O16 (mp-771993) | 0.1626 | 0.069 | 4 |
Fe3O4 (mp-715490) | 0.1467 | 0.000 | 2 |
Fe3O4 (mp-542433) | 0.1128 | 0.075 | 2 |
Fe3O4 (mp-567124) | 0.1484 | 0.017 | 2 |
Fe3O4 (mp-716052) | 0.0745 | 0.781 | 2 |
Fe3O4 (mp-715811) | 0.0231 | 0.037 | 2 |
Li4Ti3Cr3(SnO8)2 (mp-776780) | 0.2672 | 0.138 | 5 |
Li4Ti3Cr3(WO8)2 (mp-773537) | 0.2739 | 0.054 | 5 |
Li4Cr3Fe3(TeO8)2 (mp-773518) | 0.2687 | 0.054 | 5 |
Li4Cr3Fe3(SbO8)2 (mp-771925) | 0.2893 | 6.495 | 5 |
Li4Nb3V3(SnO8)2 (mp-767976) | 0.2936 | 0.129 | 5 |
Li3MnFeCo(PO4)3 (mp-764931) | 0.7186 | 0.017 | 6 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.7062 | 0.014 | 6 |
Li3MnFeCo(PO4)3 (mp-764869) | 0.7135 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764969) | 0.7122 | 0.057 | 6 |
Li3MnFeCo(PO4)3 (mp-764870) | 0.7207 | 0.466 | 6 |
Explore more synthesis descriptions for materials of composition Fe3O4.
Text computed by synthesisproject.org.
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Fe_pv O |
Final Energy/Atom-5.9581 eV |
Corrected Energy-204.8907 eV
Uncorrected energy = -166.8267 eV
Composition-based energy adjustment (-0.687 eV/atom x 16.0 atoms) = -10.9920 eV
Composition-based energy adjustment (-2.256 eV/atom x 12.0 atoms) = -27.0720 eV
Corrected energy = -204.8907 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)