Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.871 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.027 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.15 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNaLaMgWO6 |
Band Gap3.157 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP4/nmm [129] |
HallP 4ab 2ab 1ab |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 1> | 328.9 |
AlN (mp-661) | <0 0 1> | <1 0 1> | 109.6 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 314.6 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 188.4 |
AlN (mp-661) | <1 1 0> | <1 1 1> | 212.7 |
AlN (mp-661) | <1 1 1> | <1 1 1> | 141.8 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 224.7 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 134.8 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 190.7 |
Te2W (mp-22693) | <0 1 0> | <1 1 1> | 283.5 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 251.2 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 282.6 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 269.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 157.0 |
BN (mp-984) | <1 0 0> | <0 0 1> | 94.2 |
BN (mp-984) | <1 1 0> | <0 0 1> | 314.0 |
CdTe (mp-406) | <1 1 0> | <1 0 0> | 179.8 |
TeO2 (mp-2125) | <0 1 1> | <1 0 0> | 224.7 |
TeO2 (mp-2125) | <1 0 0> | <1 0 0> | 134.8 |
TeO2 (mp-2125) | <1 1 0> | <1 1 0> | 190.7 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 314.0 |
SiC (mp-7631) | <1 0 1> | <0 0 1> | 251.2 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 31.4 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 127.1 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 157.0 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 31.4 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 44.9 |
GaAs (mp-2534) | <1 1 1> | <1 0 0> | 224.7 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 157.0 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 157.0 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 219.8 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 251.2 |
GaN (mp-804) | <1 0 1> | <1 1 1> | 283.5 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 89.9 |
GaN (mp-804) | <1 1 1> | <1 0 1> | 219.3 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 282.6 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 314.0 |
C (mp-66) | <1 0 0> | <0 0 1> | 62.8 |
SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 54.8 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 134.8 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 190.7 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 157.0 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 179.8 |
GdScO3 (mp-5690) | <0 1 0> | <1 0 0> | 44.9 |
GdScO3 (mp-5690) | <1 0 0> | <1 1 1> | 141.8 |
GdScO3 (mp-5690) | <1 1 0> | <0 0 1> | 62.8 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 157.0 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 251.2 |
Mg (mp-153) | <1 0 1> | <1 1 1> | 283.5 |
Mg (mp-153) | <1 1 0> | <1 0 0> | 89.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
BaZrSe3 (mp-998350) | 0.3549 | 0.078 | 3 |
KCrF3 (mp-560547) | 0.3741 | 0.000 | 3 |
CaSiO3 (mp-3382) | 0.3661 | 0.244 | 3 |
MnNF3 (mp-1078939) | 0.3687 | 1.042 | 3 |
SrHfO3 (mp-13108) | 0.3380 | 0.033 | 3 |
BaLaMn2O6 (mp-19245) | 0.2802 | 0.113 | 4 |
BaPrMn2O6 (mp-19274) | 0.2840 | 0.031 | 4 |
BaLa(CoO3)2 (mp-24855) | 0.2489 | 0.109 | 4 |
BaNdMn2O6 (mp-25004) | 0.2919 | 0.040 | 4 |
BaNd(CoO3)2 (mp-1079144) | 0.3051 | 0.090 | 4 |
Mn4N (mp-637576) | 0.5665 | 1.992 | 2 |
Fe2O3 (mp-1068212) | 0.5574 | 0.860 | 2 |
Fe4P (mp-20885) | 0.5689 | 0.686 | 2 |
Ni4O (mp-1094082) | 0.5699 | 1.732 | 2 |
Ni4N (mp-1094090) | 0.5699 | 0.067 | 2 |
Ba6Sr2CoCu7O24 (mp-1076247) | 0.3475 | 0.092 | 5 |
Ba3SrCo(CuO4)3 (mp-1099886) | 0.3443 | 0.126 | 5 |
Ba3Sr5Co3Cu5O24 (mp-1076600) | 0.3415 | 0.116 | 5 |
Ba3Sr5Co2(CuO4)6 (mp-1076137) | 0.3301 | 0.097 | 5 |
Ba2Sr2Co(CuO4)3 (mp-1099763) | 0.3442 | 0.108 | 5 |
Na5Ca2Ce3Ti8Nb2O30 (mp-721094) | 0.3702 | 0.065 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesW: 6.2 eV |
PseudopotentialsVASP PAW: Na_pv La Mg_pv W_pv O |
Final Energy/Atom-7.0634 eV |
Corrected Energy-158.3875 eV
Uncorrected energy = -141.2675 eV
Composition-based energy adjustment (-0.687 eV/atom x 12.0 atoms) = -8.2440 eV
Composition-based energy adjustment (-4.438 eV/atom x 2.0 atoms) = -8.8760 eV
Corrected energy = -158.3875 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)