Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.750 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.010 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.39 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToGeS2 + InAgS2 |
Band Gap1.410 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCc [9] |
HallC 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 -1> | 179.8 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 -1> | 211.7 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 171.9 |
CdS (mp-672) | <1 1 0> | <1 0 1> | 150.0 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 91.7 |
CdS (mp-672) | <1 1 1> | <1 0 -1> | 105.8 |
YVO4 (mp-19133) | <1 0 1> | <1 0 -1> | 211.7 |
YVO4 (mp-19133) | <0 0 1> | <1 0 -1> | 105.8 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 91.7 |
TePb (mp-19717) | <1 0 0> | <1 0 -1> | 211.7 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 145.3 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 91.7 |
Al (mp-134) | <1 0 0> | <1 0 -1> | 211.7 |
TeO2 (mp-2125) | <0 1 0> | <1 0 0> | 275.2 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 275.2 |
C (mp-66) | <1 1 0> | <0 1 0> | 145.3 |
LaF3 (mp-905) | <1 1 0> | <1 0 0> | 91.7 |
LaF3 (mp-905) | <0 0 1> | <1 0 0> | 91.7 |
LaF3 (mp-905) | <1 0 0> | <1 0 -1> | 105.8 |
InP (mp-20351) | <1 1 1> | <1 1 -1> | 179.8 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 183.4 |
Ga2O3 (mp-886) | <1 0 -1> | <1 0 0> | 275.2 |
ZrO2 (mp-2858) | <0 0 1> | <1 0 0> | 275.2 |
Ge(Bi3O5)4 (mp-23352) | <1 1 1> | <1 1 -1> | 179.8 |
YAlO3 (mp-3792) | <0 1 0> | <1 0 0> | 275.2 |
YAlO3 (mp-3792) | <1 1 0> | <1 0 0> | 275.2 |
YAlO3 (mp-3792) | <1 0 0> | <1 0 0> | 275.2 |
CdWO4 (mp-19387) | <1 1 1> | <1 0 -1> | 105.8 |
SiC (mp-8062) | <1 1 0> | <1 0 0> | 275.2 |
ZnO (mp-2133) | <1 0 0> | <0 0 1> | 275.5 |
ZnO (mp-2133) | <1 0 1> | <1 0 0> | 275.2 |
MgF2 (mp-1249) | <1 0 1> | <1 0 0> | 183.4 |
LiAlO2 (mp-3427) | <0 0 1> | <1 0 0> | 275.2 |
LiAlO2 (mp-3427) | <1 1 0> | <1 0 0> | 91.7 |
LiAlO2 (mp-3427) | <1 1 1> | <1 0 -1> | 105.8 |
Al2O3 (mp-1143) | <0 0 1> | <1 1 -1> | 179.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cd4GeS6 (mp-5151) | 0.3147 | 0.012 | 3 |
Cd4SiSe6 (mp-17791) | 0.3259 | 0.013 | 3 |
Si(Hg2S3)2 (mp-17948) | 0.3690 | 0.013 | 3 |
Cd4GeSe6 (mp-18163) | 0.2935 | 0.018 | 3 |
Si(Hg2Se3)2 (mp-18230) | 0.3268 | 0.017 | 3 |
In2Si(AgSe3)2 (mp-640614) | 0.2104 | 0.009 | 4 |
In2Cu2SiS6 (mp-558055) | 0.3345 | 0.055 | 4 |
In2Si(AgS3)2 (mp-558407) | 0.1289 | 0.006 | 4 |
Li2CrSiO4 (mp-761657) | 0.3359 | 0.293 | 4 |
In2Ag2GeSe6 (mp-505607) | 0.1533 | 0.018 | 4 |
GeAs (mp-9548) | 0.6538 | 0.002 | 2 |
Ag3P11 (mp-27821) | 0.5392 | 0.000 | 2 |
GaTe (mp-542812) | 0.6073 | 0.003 | 2 |
CuP10 (mp-606644) | 0.6198 | 0.000 | 2 |
Cu2P7 (mp-28034) | 0.6006 | 0.000 | 2 |
Li4Mn3P3O12F (mp-762779) | 0.6866 | 0.068 | 5 |
Li4Fe3P3O12F (mp-762712) | 0.6803 | 0.057 | 5 |
Li2PWO4F (mp-25728) | 0.7283 | 0.352 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: In_d Ag Ge_d S |
Final Energy/Atom-4.0796 eV |
Corrected Energy-95.7866 eV
Uncorrected energy = -89.7506 eV
Composition-based energy adjustment (-0.503 eV/atom x 12.0 atoms) = -6.0360 eV
Corrected energy = -95.7866 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)