Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.971 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.73 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.838 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFd3m [227] |
HallF 4d 2 3 1d |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <1 0 0> | 115.8 |
C (mp-66) | <1 1 0> | <1 1 0> | 163.8 |
Mg (mp-153) | <1 1 0> | <1 0 0> | 115.8 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 0 0> | 231.7 |
KP(HO2)2 (mp-23959) | <1 0 0> | <1 0 0> | 115.8 |
PbSe (mp-2201) | <1 1 0> | <1 1 0> | 163.8 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 163.8 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 115.8 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 163.8 |
CdSe (mp-2691) | <1 1 0> | <1 1 0> | 163.8 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 163.8 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 163.8 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 163.8 |
YAlO3 (mp-3792) | <1 0 0> | <1 1 0> | 163.8 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 163.8 |
SiC (mp-8062) | <1 1 0> | <1 1 0> | 163.8 |
GaSb (mp-1156) | <1 1 0> | <1 1 0> | 163.8 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 231.7 |
SiC (mp-7631) | <1 1 0> | <1 1 0> | 163.8 |
Ge3(BiO3)4 (mp-23560) | <1 1 0> | <1 1 0> | 163.8 |
C (mp-66) | <1 0 0> | <1 0 0> | 115.8 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 0> | 231.7 |
Ga2O3 (mp-886) | <1 0 1> | <1 0 0> | 231.7 |
ZrO2 (mp-2858) | <1 0 0> | <1 0 0> | 115.8 |
YAlO3 (mp-3792) | <1 1 0> | <1 0 0> | 115.8 |
TiO2 (mp-390) | <0 0 1> | <1 0 0> | 115.8 |
ZnTe (mp-2176) | <1 1 0> | <1 1 0> | 163.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
La2Zr2O7 (mp-4974) | 0.0090 | 0.000 | 3 |
Bi2Pt2O7 (mp-23341) | 0.0064 | 0.000 | 3 |
La2Pt2O7 (mp-755026) | 0.0025 | 0.000 | 3 |
Tm2V2O7 (mp-19036) | 0.0096 | 0.083 | 3 |
Nd2Mo2O7 (mp-33803) | 0.0023 | 0.000 | 3 |
Mn2Hg2SF6 (mp-600275) | 0.2674 | 0.465 | 4 |
Zn2Hg2OF6 (mp-17972) | 0.2589 | 0.000 | 4 |
Mn2Hg2SF6 (mp-556900) | 0.2508 | 0.465 | 4 |
Ni2Hg2OF6 (mp-540834) | 0.3416 | 0.000 | 4 |
Ca2Ta2O6F (mp-14560) | 0.0600 | 0.076 | 4 |
GdTi2CdO6F (mp-695048) | 0.3220 | 0.142 | 5 |
YbTi2CdO6F (mp-677010) | 0.2654 | 0.121 | 5 |
NdTi2CdO6F (mp-677732) | 0.3052 | 0.159 | 5 |
EuTi2CdO6F (mp-684730) | 0.2736 | 0.099 | 5 |
Ca2Nd2Nb3FeO14 (mp-40206) | 0.3943 | 0.111 | 5 |
NaYbTiNbO6F (mp-684861) | 0.5454 | 0.065 | 6 |
NaPrTiNbO6F (mp-42897) | 0.5935 | 0.035 | 6 |
NaEuTiNbO6F (mp-43048) | 0.5028 | 0.021 | 6 |
NaCeTiNbO6F (mp-43055) | 0.5698 | 0.039 | 6 |
NaNdTiNbO6F (mp-43134) | 0.5930 | 0.038 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Pr_3 Sn_d O |
Final Energy/Atom-7.2677 eV |
Corrected Energy-169.5072 eV
Uncorrected energy = -159.8892 eV
Composition-based energy adjustment (-0.687 eV/atom x 14.0 atoms) = -9.6180 eV
Corrected energy = -169.5072 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)