Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.122 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.009 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.46 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToAlPO4 |
Band Gap5.618 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP3221 [154] |
HallP 32 2" |
Point Group32 |
Crystal Systemtrigonal |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | elastic energy [meV] | MCIA† [Å2] |
---|---|---|---|---|
C (mp-66) | <1 1 1> | <0 0 1> | 0.000 | 22.1 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 0.000 | 199.2 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 0.000 | 22.1 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 0.001 | 88.5 |
ZnTe (mp-2176) | <1 1 1> | <0 0 1> | 0.001 | 66.4 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 1> | 0.001 | 303.1 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 0.001 | 154.9 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 0.001 | 66.4 |
Si (mp-149) | <1 1 1> | <0 0 1> | 0.002 | 154.9 |
C (mp-66) | <1 0 0> | <0 0 1> | 0.002 | 243.4 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 0.004 | 293.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 0.007 | 199.2 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 0.008 | 66.4 |
ZrO2 (mp-2858) | <0 1 0> | <1 1 0> | 0.008 | 195.5 |
BN (mp-984) | <1 0 1> | <0 0 1> | 0.012 | 243.4 |
GaSb (mp-1156) | <1 1 1> | <0 0 1> | 0.013 | 66.4 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 0.017 | 265.6 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 0.018 | 66.4 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 0.018 | 66.4 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 0.019 | 199.2 |
BN (mp-984) | <1 0 0> | <0 0 1> | 0.020 | 154.9 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 0.021 | 66.4 |
BN (mp-984) | <0 0 1> | <0 0 1> | 0.022 | 22.1 |
ZnO (mp-2133) | <0 0 1> | <0 0 1> | 0.023 | 66.4 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 0.028 | 354.1 |
SiC (mp-8062) | <1 0 0> | <0 0 1> | 0.029 | 154.9 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 0.030 | 22.1 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 0.031 | 265.6 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 0.032 | 287.7 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 0.033 | 354.1 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 0.035 | 287.7 |
ZrO2 (mp-2858) | <1 1 -1> | <1 0 0> | 0.037 | 225.7 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 0.040 | 88.5 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 0.044 | 154.9 |
GaP (mp-2490) | <1 1 1> | <0 0 1> | 0.045 | 154.9 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 0.047 | 154.9 |
Mg (mp-153) | <1 1 0> | <1 1 0> | 0.049 | 293.2 |
CdWO4 (mp-19387) | <0 1 0> | <0 0 1> | 0.049 | 287.7 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 0.051 | 287.7 |
Ga2O3 (mp-886) | <1 0 1> | <1 0 1> | 0.052 | 181.9 |
MgF2 (mp-1249) | <1 0 1> | <0 0 1> | 0.052 | 376.2 |
ZrO2 (mp-2858) | <0 1 1> | <0 0 1> | 0.056 | 199.2 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 0.059 | 354.1 |
CaCO3 (mp-3953) | <1 1 1> | <0 0 1> | 0.060 | 154.9 |
CaCO3 (mp-3953) | <1 0 0> | <0 0 1> | 0.061 | 88.5 |
ZrO2 (mp-2858) | <1 0 -1> | <1 1 0> | 0.061 | 293.2 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 0.062 | 169.3 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 0.062 | 287.7 |
BaTiO3 (mp-5986) | <1 1 0> | <1 0 0> | 0.065 | 282.2 |
CaF2 (mp-2741) | <1 1 1> | <0 0 1> | 0.066 | 154.9 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
70 | 2 | 12 | 12 | 0 | 0 |
2 | 70 | 12 | -12 | 0 | 0 |
12 | 12 | 77 | 0 | 0 | 0 |
12 | -12 | 0 | 41 | 0 | 0 |
0 | 0 | 0 | 0 | 41 | 12 |
0 | 0 | 0 | 0 | 12 | 34 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
15.6 | -0.9 | -2.2 | -4.7 | 0.0 | 0.0 |
-0.9 | 15.6 | -2.2 | 4.7 | -0.0 | 0.0 |
-2.2 | -2.2 | 13.7 | -0.0 | -0.0 | -0.0 |
-4.7 | 4.7 | -0.0 | 27.3 | 0.0 | -0.0 |
-0.0 | -0.0 | 0.0 | 0.0 | 27.3 | -9.5 |
0.0 | 0.0 | -0.0 | -0.0 | -9.5 | 32.9 |
Shear Modulus GV36 GPa |
Bulk Modulus KV30 GPa |
Shear Modulus GR32 GPa |
Bulk Modulus KR29 GPa |
Shear Modulus GVRH34 GPa |
Bulk Modulus KVRH29 GPa |
Elastic Anisotropy0.53 |
Poisson's Ratio0.08 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
AlPO4 (mp-7848) | 0.0843 | 0.000 | 3 |
AlPO4 (mp-4051) | 0.1015 | 0.002 | 3 |
VBO4 (mp-778780) | 0.1749 | 0.000 | 3 |
AlPO4 (mp-555941) | 0.1596 | 0.011 | 3 |
AlPO4 (mp-5331) | 0.0036 | 0.009 | 3 |
CsBeAsO4 (mp-9113) | 0.6931 | 0.000 | 4 |
KSi2BO6 (mp-1019889) | 0.7245 | 0.000 | 4 |
Cs2MgSi5O12 (mp-1019610) | 0.6668 | 0.000 | 4 |
TiO2 (mp-553432) | 0.2414 | 0.049 | 2 |
SiO2 (mp-7000) | 0.2650 | 0.011 | 2 |
SiO2 (mp-12787) | 0.2941 | 0.010 | 2 |
BeF2 (mp-15951) | 0.2425 | 0.000 | 2 |
SiO2 (mp-6930) | 0.2626 | 0.010 | 2 |
Explore more synthesis descriptions for materials of composition AlPO4.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Al P O |
Final Energy/Atom-7.4787 eV |
Corrected Energy-142.8608 eV
Uncorrected energy = -134.6168 eV
Composition-based energy adjustment (-0.687 eV/atom x 12.0 atoms) = -8.2440 eV
Corrected energy = -142.8608 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)