@article{Webster1971, author = "Webster, P.J.", title = "Magnetic and chemical order in Heusler alloys containing cobalt and manganese", journal = "Journal of Physics and Chemistry of Solids", year = "1971", volume = "32", pages = "1221-1231", ASTM_id = "JPCSAW" } @article{Buschow1983, author = "Buschow, K.H.J. and van Engen, P.G. and Jongebreur, R.", title = "Magneto-optical properties of metallic ferromagnetic materials", journal = "Journal of Magnetism and Magnetic Materials", year = "1983", volume = "38", pages = "1-22", ASTM_id = "JMMMDC" } @article{Buschow1981, author = "Buschow, K.H.J. and van Engen, P.G.", title = "Magnetic and magneto-optical properties of Heusler alloys based on aluminium and gallium", journal = "Journal of Magnetism and Magnetic Materials", year = "1981", volume = "25", pages = "90-96", ASTM_id = "JMMMDC" } @article{Huang2012, author = "Huang, H.M. and Luo, S.J. and Yao, K.L.", title = "Half metallicity through wide range of lattice constants in Heusler alloys Co2 Mn Ga1-x Gex : first-principles calculations", journal = "Physica Status Solidi B - Basic Solid State Physics", year = "2012", volume = "249", pages = "840-846", ASTM_id = "PSSBBD" } @article{Wunsch1979, author = "Wunsch, K.M. and Wachtel, E.", title = "Zur Umbildung der Gitterstruktur vom B2-Typ in den L21-Typ am Beispiel von Co50 Mnx Ga50-x-Legierungen", journal = "Journal of the Less-Common Metals", year = "1979", volume = "66", pages = "13-21", ASTM_id = "JCOMAH" }