# generated using pymatgen data_Al _symmetry_space_group_name_H-M 'P 1' _cell_length_a 4.04362100 _cell_length_b 6.37428973 _cell_length_c 37.76098111 _cell_angle_alpha 89.99999479 _cell_angle_beta 90.00000000 _cell_angle_gamma 90.00000000 _symmetry_Int_Tables_number 1 _chemical_formula_structural Al _chemical_formula_sum Al58 _cell_volume 973.29728582 _cell_formula_units_Z 58 loop_ _symmetry_equiv_pos_site_id _symmetry_equiv_pos_as_xyz 1 'x, y, z' loop_ _atom_site_type_symbol _atom_site_label _atom_site_symmetry_multiplicity _atom_site_fract_x _atom_site_fract_y _atom_site_fract_z _atom_site_occupancy Al Al0 1 0.500000 0.677635 0.500000 1 Al Al1 1 0.500000 0.322365 0.000000 1 Al Al2 1 0.500000 0.102177 0.885621 1 Al Al3 1 0.500000 0.904849 0.952703 1 Al Al4 1 0.500000 0.498589 0.919337 1 Al Al5 1 0.500000 0.699807 0.851206 1 Al Al6 1 0.500000 0.899500 0.784016 1 Al Al7 1 0.500000 0.300305 0.817687 1 Al Al8 1 0.500000 0.500000 0.750000 1 Al Al9 1 0.500000 0.699695 0.682313 1 Al Al10 1 0.500000 0.095151 0.547297 1 Al Al11 1 0.500000 0.897823 0.614379 1 Al Al12 1 0.500000 0.300193 0.648794 1 Al Al13 1 0.500000 0.501411 0.580663 1 Al Al14 1 0.500000 0.100500 0.715984 1 Al Al15 1 0.500000 0.102177 0.114379 1 Al Al16 1 0.500000 0.904849 0.047297 1 Al Al17 1 0.500000 0.699807 0.148794 1 Al Al18 1 0.500000 0.498589 0.080663 1 Al Al19 1 0.500000 0.899500 0.215984 1 Al Al20 1 0.500000 0.699695 0.317687 1 Al Al21 1 0.500000 0.500000 0.250000 1 Al Al22 1 0.500000 0.300305 0.182313 1 Al Al23 1 0.500000 0.501411 0.419337 1 Al Al24 1 0.500000 0.300193 0.351206 1 Al Al25 1 0.500000 0.100500 0.284016 1 Al Al26 1 0.500000 0.095151 0.452703 1 Al Al27 1 0.500000 0.897823 0.385621 1 Al Al28 1 0.000000 0.200425 0.766851 1 Al Al29 1 0.000000 0.400410 0.699267 1 Al Al30 1 0.000000 0.599326 0.631985 1 Al Al31 1 0.000000 0.599590 0.800733 1 Al Al32 1 0.000000 0.799575 0.733149 1 Al Al33 1 0.000000 0.400674 0.868015 1 Al Al34 1 0.000000 0.401075 0.465728 1 Al Al35 1 0.000000 0.401075 0.534272 1 Al Al36 1 0.000000 0.195860 0.599367 1 Al Al37 1 0.000000 0.195860 0.400633 1 Al Al38 1 0.000000 0.999126 0.334312 1 Al Al39 1 0.000000 0.999126 0.665688 1 Al Al40 1 0.000000 0.004598 0.500000 1 Al Al41 1 0.000000 0.794163 0.563279 1 Al Al42 1 0.000000 0.794163 0.436721 1 Al Al43 1 0.000000 0.205837 0.063279 1 Al Al44 1 0.000000 0.995402 0.000000 1 Al Al45 1 0.000000 0.205837 0.936721 1 Al Al46 1 0.000000 0.598925 0.034272 1 Al Al47 1 0.000000 0.598925 0.965728 1 Al Al48 1 0.000000 0.804140 0.900633 1 Al Al49 1 0.000000 0.804140 0.099367 1 Al Al50 1 0.000000 0.000874 0.165688 1 Al Al51 1 0.000000 0.000874 0.834312 1 Al Al52 1 0.000000 0.400410 0.300733 1 Al Al53 1 0.000000 0.200425 0.233149 1 Al Al54 1 0.000000 0.599326 0.368015 1 Al Al55 1 0.000000 0.400674 0.131985 1 Al Al56 1 0.000000 0.599590 0.199267 1 Al Al57 1 0.000000 0.799575 0.266851 1