Final Magnetic Moment0.175 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.054 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.180 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.01 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2Ca + Ca2Ge + Ca |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
KCl (mp-23193) | <1 0 0> | <1 0 0> | 207.8 |
YVO4 (mp-19133) | <1 0 0> | <1 1 1> | 180.0 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 146.9 |
LaF3 (mp-905) | <0 0 1> | <1 1 1> | 180.0 |
InP (mp-20351) | <1 1 0> | <1 1 0> | 146.9 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 207.8 |
Ge(Bi3O5)4 (mp-23352) | <1 0 0> | <1 0 0> | 103.9 |
Ge(Bi3O5)4 (mp-23352) | <1 1 1> | <1 1 1> | 180.0 |
Cu (mp-30) | <1 1 0> | <1 1 0> | 146.9 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 103.9 |
LiNbO3 (mp-3731) | <1 0 0> | <1 1 0> | 146.9 |
Al (mp-134) | <1 1 0> | <1 0 0> | 207.8 |
InP (mp-20351) | <1 1 1> | <1 1 1> | 180.0 |
BaTiO3 (mp-5986) | <0 0 1> | <1 0 0> | 207.8 |
Au (mp-81) | <1 1 0> | <1 1 0> | 146.9 |
Ge(Bi3O5)4 (mp-23352) | <1 1 0> | <1 1 0> | 146.9 |
Cu (mp-30) | <1 0 0> | <1 0 0> | 103.9 |
Al2O3 (mp-1143) | <0 0 1> | <1 1 1> | 180.0 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
21 | 24 | 24 | 0 | 0 | 0 |
24 | 21 | 24 | 0 | 0 | 0 |
24 | 24 | 21 | 0 | 0 | 0 |
0 | 0 | 0 | 19 | 0 | 0 |
0 | 0 | 0 | 0 | 19 | 0 |
0 | 0 | 0 | 0 | 0 | 19 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
-212.2 | 113.2 | 113.2 | 0 | 0 | 0 |
113.2 | -212.2 | 113.2 | 0 | 0 | 0 |
113.2 | 113.2 | -212.2 | 0 | 0 | 0 |
0 | 0 | 0 | 52.5 | 0 | 0 |
0 | 0 | 0 | 0 | 52.5 | 0 |
0 | 0 | 0 | 0 | 0 | 52.5 |
Shear Modulus GV11 GPa |
Bulk Modulus KV23 GPa |
Shear Modulus GR-4 GPa |
Bulk Modulus KR23 GPa |
Shear Modulus GVRH3 GPa |
Bulk Modulus KVRH23 GPa |
Elastic Anisotropy-17.37 |
Poisson's Ratio0.43 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ZnCu2Ni (mp-30593) | 0.1125 | 0.005 | 3 |
CrCoPt2 (mp-570863) | 0.0492 | 0.000 | 3 |
GaFeNi2 (mp-1065359) | 0.0412 | 0.066 | 3 |
GaCo2Ni (mp-1018060) | 0.0157 | 0.075 | 3 |
Cr8Ni50Mo15W2 (mp-767372) | 0.2155 | 0.028 | 4 |
CrFeCoNi (mp-1012640) | 0.3608 | 0.118 | 4 |
CrFeCoNi (mp-1096923) | 0.4019 | 0.193 | 4 |
LuRu3 (mp-973652) | 0.0000 | 0.356 | 2 |
Ti3Ni (mp-981209) | 0.0000 | 0.129 | 2 |
Mg3Mo (mp-978287) | 0.0000 | 0.317 | 2 |
CuPt7 (mp-12608) | 0.0000 | 0.000 | 2 |
SbPt7 (mp-1030) | 0.0000 | 0.019 | 2 |
U (mp-1008669) | 0.0000 | 0.372 | 1 |
Pb (mp-20483) | 0.0000 | 0.000 | 1 |
Cs (mp-1055940) | 0.0000 | 0.041 | 1 |
Er (mp-10752) | 0.0000 | 0.027 | 1 |
Br (mp-998861) | 0.0000 | 0.666 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Ca_sv Ge_d |
Final Energy/Atom-2.3698 eV |
Corrected Energy-18.9581 eV
Uncorrected energy = -18.9581 eV
Corrected energy = -18.9581 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)