# generated using pymatgen data_Ag _symmetry_space_group_name_H-M 'P 1' _cell_length_a 2.91566996 _cell_length_b 9.28478205 _cell_length_c 49.57865533 _cell_angle_alpha 89.99999846 _cell_angle_beta 90.00000000 _cell_angle_gamma 71.69792565 _symmetry_Int_Tables_number 1 _chemical_formula_structural Ag _chemical_formula_sum Ag70 _cell_volume 1274.26719072 _cell_formula_units_Z 70 loop_ _symmetry_equiv_pos_site_id _symmetry_equiv_pos_as_xyz 1 'x, y, z' loop_ _atom_site_type_symbol _atom_site_label _atom_site_symmetry_multiplicity _atom_site_fract_x _atom_site_fract_y _atom_site_fract_z _atom_site_occupancy Ag Ag0 1 0.886152 0.613848 0.568202 1 Ag Ag1 1 0.221641 0.778359 0.609816 1 Ag Ag2 1 0.329758 0.170242 0.460439 1 Ag Ag3 1 0.446802 0.053198 0.404761 1 Ag Ag4 1 0.666787 0.333213 0.417914 1 Ag Ag5 1 0.118363 0.881637 0.447590 1 Ag Ag6 1 0.000109 0.499891 0.375908 1 Ag Ag7 1 0.795012 0.704988 0.500000 1 Ag Ag8 1 0.446802 0.053198 0.595239 1 Ag Ag9 1 0.329758 0.170242 0.539561 1 Ag Ag10 1 0.549070 0.450930 0.472399 1 Ag Ag11 1 0.549070 0.450930 0.527601 1 Ag Ag12 1 0.666787 0.333213 0.582086 1 Ag Ag13 1 0.118363 0.881637 0.552410 1 Ag Ag14 1 0.886152 0.613848 0.431798 1 Ag Ag15 1 0.221641 0.778359 0.390184 1 Ag Ag16 1 0.779001 0.220999 0.637675 1 Ag Ag17 1 0.111270 0.388730 0.679930 1 Ag Ag18 1 0.888499 0.111501 0.693945 1 Ag Ag19 1 0.222186 0.277814 0.736019 1 Ag Ag20 1 0.666324 0.833676 0.708015 1 Ag Ag21 1 0.555603 0.944397 0.651885 1 Ag Ag22 1 0.333103 0.666897 0.665992 1 Ag Ag23 1 0.000109 0.499891 0.624092 1 Ag Ag24 1 0.444523 0.555477 0.721988 1 Ag Ag25 1 0.000000 0.000000 0.750000 1 Ag Ag26 1 0.555477 0.444523 0.221988 1 Ag Ag27 1 0.333676 0.166324 0.208015 1 Ag Ag28 1 0.000000 0.000000 0.250000 1 Ag Ag29 1 0.888730 0.611270 0.179930 1 Ag Ag30 1 0.220999 0.779001 0.137675 1 Ag Ag31 1 0.779001 0.220999 0.362325 1 Ag Ag32 1 0.111270 0.388730 0.320070 1 Ag Ag33 1 0.333103 0.666897 0.334008 1 Ag Ag34 1 0.444523 0.555477 0.278012 1 Ag Ag35 1 0.555603 0.944397 0.348115 1 Ag Ag36 1 0.666324 0.833676 0.291985 1 Ag Ag37 1 0.888499 0.111501 0.306055 1 Ag Ag38 1 0.222186 0.277814 0.263981 1 Ag Ag39 1 0.666897 0.333103 0.165992 1 Ag Ag40 1 0.444397 0.055603 0.151885 1 Ag Ag41 1 0.999891 0.500109 0.124092 1 Ag Ag42 1 0.111501 0.888499 0.193945 1 Ag Ag43 1 0.777814 0.722186 0.236019 1 Ag Ag44 1 0.778359 0.221641 0.890184 1 Ag Ag45 1 0.113848 0.386152 0.931798 1 Ag Ag46 1 0.444397 0.055603 0.848115 1 Ag Ag47 1 0.333676 0.166324 0.791985 1 Ag Ag48 1 0.666897 0.333103 0.834008 1 Ag Ag49 1 0.555477 0.444523 0.778012 1 Ag Ag50 1 0.111501 0.888499 0.806055 1 Ag Ag51 1 0.888730 0.611270 0.820070 1 Ag Ag52 1 0.777814 0.722186 0.763981 1 Ag Ag53 1 0.553198 0.946802 0.904761 1 Ag Ag54 1 0.220999 0.779001 0.862325 1 Ag Ag55 1 0.204988 0.295012 0.000000 1 Ag Ag56 1 0.553198 0.946802 0.095239 1 Ag Ag57 1 0.670242 0.829758 0.039561 1 Ag Ag58 1 0.450930 0.549070 0.027601 1 Ag Ag59 1 0.450930 0.549070 0.972399 1 Ag Ag60 1 0.333213 0.666787 0.082086 1 Ag Ag61 1 0.670242 0.829758 0.960439 1 Ag Ag62 1 0.333213 0.666787 0.917914 1 Ag Ag63 1 0.881637 0.118363 0.052410 1 Ag Ag64 1 0.113848 0.386152 0.068202 1 Ag Ag65 1 0.778359 0.221641 0.109816 1 Ag Ag66 1 0.881637 0.118363 0.947590 1 Ag Ag67 1 0.999891 0.500109 0.875908 1 Ag Ag68 1 0.996176 0.003824 0.000000 1 Ag Ag69 1 0.003824 0.996176 0.500000 1