Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.263 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.097 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.00 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToK2CN2 + KC2N3 + C + Pd |
Band Gap3.899 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
| substrate material | substrate orientation | film orientation | MCIA† [Å2] |
|---|---|---|---|
| AlN (mp-661) | <1 0 0> | <0 1 0> | 305.2 |
| AlN (mp-661) | <1 0 1> | <0 0 1> | 314.0 |
| CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 244.2 |
| CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 174.4 |
| CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 104.7 |
| BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 279.1 |
| BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 279.1 |
| BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 69.8 |
| GaN (mp-804) | <0 0 1> | <0 0 1> | 279.1 |
| GaN (mp-804) | <1 0 0> | <0 1 0> | 305.2 |
| GaN (mp-804) | <1 0 1> | <0 0 1> | 279.1 |
| SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 279.1 |
| SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 348.8 |
| SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 305.2 |
| KCl (mp-23193) | <1 0 0> | <0 0 1> | 279.1 |
| KCl (mp-23193) | <1 1 0> | <0 0 1> | 279.1 |
| KCl (mp-23193) | <1 1 1> | <0 0 1> | 69.8 |
| DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 314.0 |
| DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 174.4 |
| DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 139.5 |
| DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 244.2 |
| InAs (mp-20305) | <1 0 0> | <0 0 1> | 279.1 |
| InAs (mp-20305) | <1 1 0> | <0 0 1> | 279.1 |
| KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 314.0 |
| KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 174.4 |
| CdS (mp-672) | <1 0 0> | <0 0 1> | 314.0 |
| CdS (mp-672) | <1 0 1> | <1 0 1> | 228.0 |
| CdS (mp-672) | <1 1 0> | <0 1 0> | 305.2 |
| LiF (mp-1138) | <1 0 0> | <1 1 0> | 247.9 |
| Te2W (mp-22693) | <0 0 1> | <0 0 1> | 244.2 |
| Te2W (mp-22693) | <0 1 0> | <0 0 1> | 279.1 |
| YVO4 (mp-19133) | <0 0 1> | <0 1 0> | 305.2 |
| TePb (mp-19717) | <1 1 1> | <1 0 0> | 215.8 |
| Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 279.1 |
| Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 279.1 |
| Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 279.1 |
| Te2Mo (mp-602) | <1 1 1> | <0 1 1> | 281.2 |
| Ag (mp-124) | <1 1 1> | <0 0 1> | 279.1 |
| Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 34.9 |
| Bi2Te3 (mp-34202) | <1 0 0> | <0 0 1> | 139.5 |
| BN (mp-984) | <0 0 1> | <0 0 1> | 174.4 |
| BN (mp-984) | <1 0 0> | <0 0 1> | 139.5 |
| BN (mp-984) | <1 0 1> | <0 0 1> | 314.0 |
| BN (mp-984) | <1 1 0> | <0 0 1> | 34.9 |
| BN (mp-984) | <1 1 1> | <0 1 0> | 305.2 |
| LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 69.8 |
| LiNbO3 (mp-3731) | <1 0 0> | <1 0 0> | 215.8 |
| LiNbO3 (mp-3731) | <1 0 1> | <1 0 1> | 228.0 |
| LiNbO3 (mp-3731) | <1 1 0> | <1 1 0> | 124.0 |
| Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 279.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
| material | dissimilarity | Ehull | # of elements |
|---|---|---|---|
| MgAlF5 (mp-1025166) | 0.6993 | 0.547 | 3 |
| Pt(NCl)2 (mp-1078605) | 0.7409 | 0.935 | 3 |
| K2Ni(CN)4 (mp-7827) | 0.1997 | 0.084 | 4 |
| K2Pt(CN)4 (mp-637196) | 0.4837 | 0.030 | 4 |
| Tl2Ni(CN)4 (mp-569704) | 0.7144 | 0.128 | 4 |
| XeF3 (mp-561153) | 0.5288 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: K_sv Pd C N |
Final Energy/Atom-7.1821 eV |
Corrected Energy-160.8946 eV
Uncorrected energy = -158.0066 eV
Composition-based energy adjustment (-0.361 eV/atom x 8.0 atoms) = -2.8880 eV
Corrected energy = -160.8946 eV
|
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)