Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.726 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.35 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap3.666 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3 [148] |
Hall-R 3 |
Point Group3 |
Crystal Systemtrigonal |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 78.8 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 59.1 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 374.2 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 334.8 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 98.5 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 236.3 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 59.1 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 78.8 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 256.0 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 289.3 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 374.2 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 256.0 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 250.6 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 256.0 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 98.5 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 236.3 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 59.1 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 98.5 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 137.9 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 256.0 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 59.1 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 334.8 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 236.3 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 275.7 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 98.5 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 98.5 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 256.0 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 334.8 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 217.0 |
Te2W (mp-22693) | <1 0 0> | <1 0 0> | 289.3 |
Te2W (mp-22693) | <1 1 0> | <1 0 0> | 217.0 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 177.3 |
YVO4 (mp-19133) | <1 1 1> | <1 1 0> | 250.6 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 315.1 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 315.1 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 78.8 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 78.8 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 217.0 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 137.9 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 98.5 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 256.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 236.3 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 236.3 |
BN (mp-984) | <0 0 1> | <0 0 1> | 137.9 |
BN (mp-984) | <1 1 0> | <0 0 1> | 256.0 |
BN (mp-984) | <1 1 1> | <0 0 1> | 236.3 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 315.1 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 59.1 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 78.8 |
Al (mp-134) | <1 0 0> | <0 0 1> | 98.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
3.56 | 0.00 | 0.00 |
0.00 | 3.56 | 0.00 |
0.00 | 0.00 | 3.01 |
Dielectric Tensor εij (total) |
||
---|---|---|
9.12 | 0.00 | 0.00 |
0.00 | 9.12 | 0.00 |
0.00 | 0.00 | 7.96 |
Polycrystalline dielectric constant
εpoly∞
3.38
|
Polycrystalline dielectric constant
εpoly
8.73
|
Refractive Index n1.84 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
TiBO3 (mp-9716) | 0.0690 | 0.073 | 3 |
MnBO3 (mp-761288) | 0.0661 | 0.041 | 3 |
VBO3 (mp-18946) | 0.0684 | 0.000 | 3 |
FeBO3 (mp-19097) | 0.0697 | 0.000 | 3 |
ScBO3 (mp-8697) | 0.0700 | 0.000 | 3 |
LiMn(CO3)2 (mp-769558) | 0.1495 | 0.177 | 4 |
LiV(CO3)2 (mp-762019) | 0.1581 | 0.000 | 4 |
LiCr(CO3)2 (mp-770839) | 0.1725 | 0.000 | 4 |
LiFe(CO3)2 (mp-768029) | 0.1549 | 0.000 | 4 |
MnSn(BO3)2 (mp-25012) | 0.1608 | 0.000 | 4 |
SiH12C2(NF)6 (mp-697253) | 0.6887 | 0.000 | 5 |
TiH12C2(NF)6 (mp-696940) | 0.7289 | 0.000 | 5 |
Run TypeGGA |
Energy Cutoff700 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mg_pv Sn_d B O |
Final Energy/Atom-7.1685 eV |
Corrected Energy-75.8067 eV
Uncorrected energy = -71.6847 eV
Composition-based energy adjustment (-0.687 eV/atom x 6.0 atoms) = -4.1220 eV
Corrected energy = -75.8067 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)