Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-4.183 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.69 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap6.624 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | elastic energy [meV] | MCIA† [Å2] |
---|---|---|---|---|
WS2 (mp-224) | <0 0 1> | <1 1 1> | 0.000 | 273.5 |
MoS2 (mp-1434) | <0 0 1> | <1 1 1> | 0.000 | 273.5 |
LiAlO2 (mp-3427) | <0 0 1> | <1 0 0> | 0.000 | 355.3 |
Y3Fe5O12 (mp-19648) | <1 0 0> | <1 0 0> | 0.000 | 157.9 |
C (mp-48) | <0 0 1> | <1 1 1> | 0.002 | 68.4 |
Fe2O3 (mp-24972) | <0 0 1> | <1 1 1> | 0.003 | 68.4 |
Te2Mo (mp-602) | <1 0 0> | <1 1 1> | 0.004 | 273.5 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 1> | 0.004 | 68.4 |
MgF2 (mp-1249) | <0 0 1> | <1 0 0> | 0.009 | 197.4 |
Mg (mp-153) | <0 0 1> | <1 1 1> | 0.010 | 273.5 |
TiO2 (mp-2657) | <1 1 1> | <1 1 1> | 0.011 | 205.1 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 0.012 | 315.8 |
Cu (mp-30) | <1 1 1> | <1 1 1> | 0.015 | 68.4 |
Cu (mp-30) | <1 1 0> | <1 1 0> | 0.015 | 55.8 |
TbScO3 (mp-31119) | <1 1 0> | <1 0 0> | 0.024 | 315.8 |
Au (mp-81) | <1 1 0> | <1 1 0> | 0.028 | 223.3 |
Au (mp-81) | <1 0 0> | <1 0 0> | 0.028 | 157.9 |
Ga2O3 (mp-886) | <1 0 0> | <1 1 1> | 0.031 | 273.5 |
ZnO (mp-2133) | <1 0 1> | <1 1 0> | 0.032 | 279.1 |
InSb (mp-20012) | <1 0 0> | <1 0 0> | 0.035 | 355.3 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 0.037 | 315.8 |
CeO2 (mp-20194) | <1 1 1> | <1 1 1> | 0.037 | 205.1 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 0.037 | 167.5 |
ZrO2 (mp-2858) | <0 0 1> | <1 0 0> | 0.039 | 355.3 |
Si (mp-149) | <1 1 1> | <1 1 1> | 0.041 | 205.1 |
Si (mp-149) | <1 1 0> | <1 1 0> | 0.041 | 167.5 |
ZnO (mp-2133) | <1 1 0> | <1 1 0> | 0.043 | 335.0 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 0.045 | 355.3 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 0.050 | 315.8 |
C (mp-66) | <1 0 0> | <1 0 0> | 0.053 | 315.8 |
ZnO (mp-2133) | <1 1 1> | <1 1 0> | 0.062 | 223.3 |
Ni (mp-23) | <1 1 0> | <1 1 0> | 0.066 | 335.0 |
Ni (mp-23) | <1 1 1> | <1 1 1> | 0.069 | 273.5 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 0.070 | 157.9 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 0.072 | 197.4 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 0.072 | 223.3 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 0.073 | 157.9 |
BaTiO3 (mp-5986) | <0 0 1> | <1 0 0> | 0.082 | 79.0 |
Ga2O3 (mp-886) | <1 1 0> | <1 1 0> | 0.084 | 223.3 |
LiF (mp-1138) | <1 1 1> | <1 1 1> | 0.084 | 205.1 |
SrTiO3 (mp-4651) | <1 1 0> | <1 0 0> | 0.085 | 315.8 |
GaSe (mp-1943) | <0 0 1> | <1 1 1> | 0.097 | 205.1 |
CdWO4 (mp-19387) | <0 0 1> | <1 1 1> | 0.097 | 273.5 |
SiC (mp-7631) | <0 0 1> | <1 1 0> | 0.099 | 167.5 |
C (mp-48) | <1 0 1> | <1 1 0> | 0.100 | 335.0 |
SiC (mp-11714) | <0 0 1> | <1 1 0> | 0.103 | 167.5 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 0.106 | 315.8 |
Te2W (mp-22693) | <1 0 1> | <1 0 0> | 0.106 | 197.4 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 0.113 | 111.7 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 0.118 | 315.8 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
87 | 38 | 38 | 0 | 0 | 0 |
38 | 87 | 38 | 0 | 0 | 0 |
38 | 38 | 87 | 0 | 0 | 0 |
0 | 0 | 0 | 24 | 0 | 0 |
0 | 0 | 0 | 0 | 24 | 0 |
0 | 0 | 0 | 0 | 0 | 24 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
15.7 | -4.8 | -4.8 | 0 | 0 | 0 |
-4.8 | 15.7 | -4.8 | 0 | 0 | 0 |
-4.8 | -4.8 | 15.7 | 0 | 0 | 0 |
0 | 0 | 0 | 42 | 0 | 0 |
0 | 0 | 0 | 0 | 42 | 0 |
0 | 0 | 0 | 0 | 0 | 42 |
Shear Modulus GV24 GPa |
Bulk Modulus KV54 GPa |
Shear Modulus GR24 GPa |
Bulk Modulus KR54 GPa |
Shear Modulus GVRH24 GPa |
Bulk Modulus KVRH54 GPa |
Elastic Anisotropy0.00 |
Poisson's Ratio0.31 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
2.32 | 0.00 | -0.00 |
0.00 | 2.32 | -0.00 |
-0.00 | -0.00 | 2.32 |
Dielectric Tensor εij (total) |
||
---|---|---|
8.34 | 0.00 | -0.00 |
0.00 | 8.34 | -0.00 |
-0.00 | -0.00 | 8.34 |
Polycrystalline dielectric constant
εpoly∞
2.32
|
Polycrystalline dielectric constant
εpoly
8.34
|
Refractive Index n1.52 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LuNiSb (mp-20185) | 0.0000 | 0.000 | 3 |
ZnFeSb (mp-20768) | 0.0000 | 0.477 | 3 |
MnSbPd (mp-4142) | 0.0000 | 0.485 | 3 |
ZrNiSn (mp-30806) | 0.0000 | 0.759 | 3 |
HoSbPt (mp-16376) | 0.0000 | 0.000 | 3 |
K2O (mp-971) | 0.0000 | 0.000 | 2 |
LaH2 (mp-24153) | 0.0000 | 0.000 | 2 |
AsRh2 (mp-2302) | 0.0000 | 0.000 | 2 |
NpO2 (mp-2616) | 0.0000 | 0.000 | 2 |
Sn2Ir (mp-2083) | 0.0000 | 0.000 | 2 |
Explore more synthesis descriptions for materials of composition BaF2.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff700 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv F |
Final Energy/Atom-5.7700 eV |
Corrected Energy-18.2339 eV
Uncorrected energy = -17.3099 eV
Composition-based energy adjustment (-0.462 eV/atom x 2.0 atoms) = -0.9240 eV
Corrected energy = -18.2339 eV
|