Final Magnetic Moment0.029 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.418 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.129 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.36 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTe2Mo + Te2W + WS2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP6m2 [187] |
HallP 6 2 |
Point Group6m2 |
Crystal Systemhexagonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <0 0 1> | 71.1 |
C (mp-48) | <1 0 0> | <0 0 1> | 254.1 |
C (mp-48) | <1 1 0> | <0 0 1> | 243.9 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 254.1 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 122.0 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 162.6 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 162.6 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 284.6 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 91.5 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 284.6 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 193.1 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 182.9 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 203.3 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 193.1 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 243.9 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 243.9 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 108.5 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 264.3 |
CdWO4 (mp-19387) | <0 1 1> | <0 0 1> | 254.1 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 132.1 |
CdWO4 (mp-19387) | <1 0 1> | <0 0 1> | 223.6 |
CdWO4 (mp-19387) | <1 1 1> | <0 0 1> | 315.1 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 284.6 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 284.6 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 61.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 71.1 |
BN (mp-984) | <0 0 1> | <0 0 1> | 71.1 |
BN (mp-984) | <1 1 0> | <0 0 1> | 274.4 |
BN (mp-984) | <1 1 1> | <0 0 1> | 274.4 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 162.6 |
Al (mp-134) | <1 0 0> | <0 0 1> | 182.9 |
Al (mp-134) | <1 1 0> | <0 0 1> | 203.3 |
Al (mp-134) | <1 1 1> | <0 0 1> | 193.1 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 315.1 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 193.1 |
CdTe (mp-406) | <1 1 1> | <0 0 1> | 315.1 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 71.1 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 325.2 |
LiTaO3 (mp-3666) | <1 0 1> | <0 0 1> | 315.1 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 91.5 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 213.4 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 152.5 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 325.2 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 193.1 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 325.2 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 162.6 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 284.6 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 172.8 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 274.4 |
Al2O3 (mp-1143) | <0 0 1> | <0 0 1> | 132.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
TeMoS (mp-1030461) | 0.0998 | 0.078 | 3 |
Te3Mo2S (mp-1030274) | 0.0791 | 0.060 | 3 |
Te3W2S (mp-1028755) | 0.0744 | 0.083 | 3 |
Te4W3S2 (mp-1026362) | 0.0085 | 0.092 | 3 |
Te4Mo3S2 (mp-1025769) | 0.0113 | 0.070 | 3 |
Te2Mo2SeS (mp-1030459) | 0.0461 | 0.055 | 4 |
Te2W2SeS (mp-1028590) | 0.0553 | 0.075 | 4 |
Te4Mo2WS2 (mp-1025743) | 0.0381 | 0.120 | 4 |
Te4Mo(WS)2 (mp-1025710) | 0.0113 | 0.083 | 4 |
Te4Mo2WS2 (mp-1025654) | 0.0142 | 0.074 | 4 |
WS2 (mp-1028441) | 0.2761 | 0.001 | 2 |
MoS2 (mp-1025874) | 0.2784 | 0.001 | 2 |
MoSe2 (mp-1025799) | 0.2782 | 0.000 | 2 |
WS2 (mp-1025571) | 0.2761 | 0.001 | 2 |
MoS2 (mp-1027525) | 0.2773 | 0.001 | 2 |
Te4Mo3W(SeS)2 (mp-1030450) | 0.0512 | 0.082 | 5 |
Te4Mo3W(SeS)2 (mp-1030404) | 0.0510 | 0.116 | 5 |
Te4Mo3W(SeS)2 (mp-1030284) | 0.0476 | 0.098 | 5 |
Te2MoWSeS (mp-1029213) | 0.0524 | 0.083 | 5 |
Te2MoWSeS (mp-1028471) | 0.0510 | 0.138 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Te Mo_pv W_pv S |
Final Energy/Atom-6.6719 eV |
Corrected Energy-62.7412 eV
Uncorrected energy = -60.0472 eV
Composition-based energy adjustment (-0.503 eV/atom x 2.0 atoms) = -1.0060 eV
Composition-based energy adjustment (-0.422 eV/atom x 4.0 atoms) = -1.6880 eV
Corrected energy = -62.7412 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)