Final Magnetic Moment0.004 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.859 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density12.46 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mmm [139] |
Hall-I 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
| substrate material | substrate orientation | film orientation | MCIA† [Å2] |
|---|---|---|---|
| C (mp-48) | <0 0 1> | <0 0 1> | 112.7 |
| C (mp-48) | <1 0 0> | <1 0 0> | 137.1 |
| C (mp-48) | <1 0 1> | <0 0 1> | 211.3 |
| C (mp-48) | <1 1 0> | <0 0 1> | 239.5 |
| C (mp-48) | <1 1 1> | <0 0 1> | 310.0 |
| LaAlO3 (mp-2920) | <0 0 1> | <1 1 0> | 48.5 |
| LaAlO3 (mp-2920) | <1 0 1> | <1 1 0> | 145.4 |
| LaAlO3 (mp-2920) | <1 1 0> | <1 0 0> | 239.9 |
| LaAlO3 (mp-2920) | <1 1 1> | <1 0 0> | 239.9 |
| AlN (mp-661) | <0 0 1> | <0 0 1> | 42.3 |
| AlN (mp-661) | <1 0 0> | <1 0 0> | 137.1 |
| AlN (mp-661) | <1 0 1> | <0 0 1> | 197.3 |
| AlN (mp-661) | <1 1 0> | <1 1 0> | 242.3 |
| AlN (mp-661) | <1 1 1> | <1 1 1> | 201.9 |
| CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 28.2 |
| CeO2 (mp-20194) | <1 1 0> | <1 1 1> | 201.9 |
| CeO2 (mp-20194) | <1 1 1> | <1 0 1> | 148.2 |
| GaAs (mp-2534) | <1 0 0> | <0 0 1> | 126.8 |
| BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 239.9 |
| BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 171.4 |
| SiO2 (mp-6930) | <0 0 1> | <1 0 1> | 259.4 |
| SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 111.2 |
| KCl (mp-23193) | <1 0 0> | <1 1 0> | 242.3 |
| KCl (mp-23193) | <1 1 0> | <1 0 0> | 171.4 |
| KCl (mp-23193) | <1 1 1> | <1 1 0> | 145.4 |
| DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 242.3 |
| DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 290.8 |
| DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 253.6 |
| DyScO3 (mp-31120) | <1 0 1> | <1 0 1> | 111.2 |
| DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 126.8 |
| InAs (mp-20305) | <1 0 0> | <0 0 1> | 183.2 |
| InAs (mp-20305) | <1 1 1> | <0 0 1> | 338.2 |
| ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 126.8 |
| ZnSe (mp-1190) | <1 1 1> | <1 1 0> | 339.3 |
| KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 126.8 |
| KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 310.0 |
| KTaO3 (mp-3614) | <1 1 1> | <1 0 1> | 111.2 |
| InP (mp-20351) | <1 0 0> | <0 0 1> | 70.4 |
| InP (mp-20351) | <1 1 0> | <1 0 1> | 259.4 |
| Te2W (mp-22693) | <0 0 1> | <1 1 1> | 201.9 |
| Te2W (mp-22693) | <0 1 1> | <1 0 1> | 296.4 |
| Te2W (mp-22693) | <1 0 0> | <0 0 1> | 281.8 |
| CdWO4 (mp-19387) | <0 0 1> | <1 0 0> | 274.2 |
| CdWO4 (mp-19387) | <0 1 0> | <1 0 0> | 239.9 |
| CdWO4 (mp-19387) | <0 1 1> | <1 0 0> | 274.2 |
| CdWO4 (mp-19387) | <1 0 0> | <1 1 0> | 96.9 |
| CdWO4 (mp-19387) | <1 0 1> | <1 0 0> | 137.1 |
| CdWO4 (mp-19387) | <1 1 1> | <0 0 1> | 324.1 |
| TePb (mp-19717) | <1 0 0> | <1 0 0> | 171.4 |
| TePb (mp-19717) | <1 1 0> | <1 0 0> | 239.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
| material | dissimilarity | Ehull | # of elements |
|---|---|---|---|
| LaSb2Au (mp-675224) | 0.1781 | 0.286 | 3 |
| ErAu2 (mp-2466) | 0.0219 | 0.000 | 2 |
| HoAu2 (mp-990) | 0.0310 | 0.000 | 2 |
| TmAu2 (mp-560) | 0.0287 | 0.000 | 2 |
| Si2W (mp-1620) | 0.0055 | 0.000 | 2 |
| YbAu2 (mp-1668) | 0.0234 | 0.000 | 2 |
| Si (mp-1056579) | 0.1905 | 0.484 | 1 |
| Sc (mp-601273) | 0.2486 | 0.128 | 1 |
| Pa (mp-62) | 0.0560 | 0.027 | 1 |
| Pr (mp-1056311) | 0.4250 | 0.096 | 1 |
| Sn (mp-55) | 0.3123 | 0.047 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Y_sv Au |
Final Energy/Atom-5.1966 eV |
Corrected Energy-15.5899 eV
Uncorrected energy = -15.5899 eV
Corrected energy = -15.5899 eV
|
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)