Final Magnetic Moment0.157 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-0.376 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.226 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.99 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCrN + N2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <0 0 1> | 226.8 |
C (mp-48) | <1 0 1> | <0 1 0> | 239.4 |
C (mp-48) | <1 1 1> | <0 0 1> | 198.5 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 143.6 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 56.7 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 170.1 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 141.8 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 302.7 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 143.6 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 260.5 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 1> | 325.6 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 56.7 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 141.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 311.9 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 191.5 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 141.8 |
InP (mp-20351) | <1 1 0> | <1 0 1> | 195.4 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 283.6 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 226.8 |
BN (mp-984) | <1 0 0> | <0 0 1> | 198.5 |
Al (mp-134) | <1 1 0> | <0 1 1> | 278.2 |
Al (mp-134) | <1 1 1> | <0 1 0> | 191.5 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 1> | 260.5 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 198.5 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 0> | 335.1 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 1> | 222.6 |
TeO2 (mp-2125) | <0 1 1> | <0 0 1> | 311.9 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 198.5 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 141.8 |
MgO (mp-1265) | <1 1 0> | <1 0 0> | 175.9 |
TiO2 (mp-2657) | <1 1 0> | <1 0 1> | 195.4 |
YVO4 (mp-19133) | <1 1 0> | <0 1 0> | 191.5 |
Mg (mp-153) | <1 1 0> | <1 0 1> | 260.5 |
Al2O3 (mp-1143) | <0 0 1> | <0 0 1> | 198.5 |
Al2O3 (mp-1143) | <1 0 1> | <0 1 0> | 335.1 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 141.8 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 255.2 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 198.5 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 260.5 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 198.5 |
TbScO3 (mp-31119) | <0 1 1> | <1 0 1> | 325.6 |
TbScO3 (mp-31119) | <1 0 0> | <0 0 1> | 141.8 |
LiNbO3 (mp-3731) | <1 1 0> | <0 0 1> | 255.2 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 1> | 65.1 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 56.7 |
LaF3 (mp-905) | <1 1 0> | <0 0 1> | 283.6 |
LiAlO2 (mp-3427) | <1 0 0> | <0 0 1> | 198.5 |
LiAlO2 (mp-3427) | <1 0 1> | <1 1 0> | 302.7 |
NdGaO3 (mp-3196) | <0 1 0> | <0 0 1> | 283.6 |
NdGaO3 (mp-3196) | <0 1 1> | <1 0 1> | 325.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mn2GeS4 (mp-621925) | 0.1349 | 0.014 | 3 |
Mg2GeS4 (mp-17441) | 0.1080 | 0.000 | 3 |
Li2ZnCl4 (mp-23416) | 0.1422 | 0.013 | 3 |
Lu2ZnS4 (mp-18332) | 0.1256 | 0.001 | 3 |
Tm2ZnS4 (mp-17043) | 0.1269 | 0.016 | 3 |
CaYbInS4 (mp-541277) | 0.1590 | 0.166 | 4 |
Li2V3WO8 (mp-775204) | 0.2483 | 0.064 | 4 |
Li2Fe3SbO8 (mp-772280) | 0.2528 | 0.000 | 4 |
Li2V3SbO8 (mp-774145) | 0.2527 | 0.010 | 4 |
CaYbInSe4 (mp-541276) | 0.1346 | 0.159 | 4 |
Fe3O4 (mp-715491) | 0.3438 | 0.017 | 2 |
Mn3N4 (mp-1080204) | 0.2555 | 0.172 | 2 |
Fe3O4 (mp-650112) | 0.3470 | 0.060 | 2 |
Fe3O4 (mp-715558) | 0.3482 | 0.785 | 2 |
Fe3O4 (mp-716052) | 0.3473 | 0.781 | 2 |
Li4Ti3Ni2Sn3O16 (mp-767702) | 0.2642 | 0.109 | 5 |
Li4Cr3Fe2Sn3O16 (mp-775748) | 0.2715 | 0.615 | 5 |
Li4V3Fe2Sn3O16 (mp-779746) | 0.2636 | 0.051 | 5 |
Li4Ti3Fe3(CuO8)2 (mp-763962) | 0.2709 | 6.078 | 5 |
Li4Ti3Cr2Fe3O16 (mp-771902) | 0.2704 | 0.088 | 5 |
Li3MnFeCo(PO4)3 (mp-764931) | 0.5952 | 0.017 | 6 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.5861 | 0.014 | 6 |
Li3MnFeCo(PO4)3 (mp-764869) | 0.5882 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764969) | 0.5877 | 0.057 | 6 |
Li3MnFeCo(PO4)3 (mp-764870) | 0.5944 | 0.466 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Cr_pv N |
Final Energy/Atom-9.0573 eV |
Corrected Energy-259.3812 eV
Uncorrected energy = -253.6052 eV
Composition-based energy adjustment (-0.361 eV/atom x 16.0 atoms) = -5.7760 eV
Corrected energy = -259.3812 eV
|